Copper Alloying Tablets (Cu75%/80%/85%)
HomeHome > Products > Additives for Non-ferrous Alloys > Copper Alloying Tablets (Cu75%/80%/85%)
Copper Alloying Tablets (Cu75%/80%/85%)

Copper Alloying Tablets (Cu75%/80%/85%)

Aluminium alloying tablets Application: Used to ajust the content of Manganese,Iron,Chromium,Titanium,Copper or Nickel e
Basic Info.
Model NO. Cu Tablets
Packing Normal or Neutral-Packing
Lead Time Within 10-15 Days
Transport Package 20kg in a Cardboard Box
Specification 75%, 80%, 85%, 90%
Trademark DongSheng
Origin China
Production Capacity 500mt/Month
Product Description
Aluminium alloying tablets
ProductPercentage of elementSpecification
Manganese tabletMn :75%,80%,85%,90%,93%1) Balance with pure Al powder or Non-hygroscopic(Sodium free) fluxes.
2) Size: Tablet: 500g-1333g/tablet.
Mini-tablet:50g-200g/mini-tablet
3) Validity period: 8 months
4) Recovery rate >95%
Iron tabletFe :75%,80%,85%,90%,97%
Titanium tabletTi : 75%,80%,85%
Chromium tabletCr :75%,80%,85%
Nickel tabletNi : 75%,80%,85%
Copper tabletCu :75%,80%
Fast melting Silicon Si : 95%
PackagingTablet: 2-4 tablets wrapped with aluminium foil, 20kg/cardboard box, 1,000kg/plywood pallet.
Mini-tablet: 10kg/paper bag , 1,000kg/plywood case.
RemarkOther weight and packaging can be produced upon customer's request.

Application:
Used to ajust the content of Manganese,Iron,Chromium,Titanium,Copper or Nickel element in the manufacturer of high quality aluminium alloys.
Usage:
1. Tablets can be added directly to the melting furnace before refining , molten aluminum temperature required: 720-750 °C
2. Calculate addition amount of tablets.
3. Put tablets into molten aluminum dispersedly after skimming away the surface dross, close the furnace door and keep 10-20 minutes.
4. Stir completely for 10 minutes, refining for 15 minutes and drossing off to get needed alloy.

Alloying tablets:
Master alloys:
Others: